Technical Data
Particle development – Model RD-319*
Test Standard Used: JIS-B-9923 (Japanese Standard)
Testing Equipment: RION KC-18
Electrostatic Discharge Test – Model
RD -319*
Particles/m 3
Surface Resistance( Ω ) |
Test Standard |
Before/After Washes |
Resistance |
Test Condition |
Wash Condition |
ASTM D257-1999 |
Before Washes |
2.5x10e 6 |
500V, 60 Sec., 20 ± 2 ° C, 65 ±2%RH |
N/A |
After Washes |
2.5x10e 6 |
AATCC135, Normal Cycle, 40 ° C, Screen Dry |
JIS L1094-1097 |
After Washes |
4.0x10e 6 |
1000V, 20 ° C, 40%RH |
Chemical Resistance Test – Model
RD-319*
Test Condition |
Chemical |
Result |
- Drop 5ml of each chemical on the glove surface.
- Wait 24 hrs. at room temperature.
- Observe if any swelling occurred.
|
Distilled Water |
No Swelling |
Hydro Chloric Acid 10% |
No Swelling |
Sulfuric Acid 10% |
No Swelling |
Acetic Acid 10% |
No Swelling |
NaOH 10% |
No Swelling |
Ammonia 10% |
No Swelling |
Mechanical Properties Comparison(RD-319 vs. Ansell Edmont HyFlex® SC*
*
All the tests were performed at the certified Korean and
Japanese test facilities. The test results are deemed reliable
and valid, but not guaranteed.